How to conduct carburizing?
Carburizing heat treatment may contain double hardening followed by low temperature tempering to ensure high hardness in surface layer
Carburizing followed by heat treatment results in surface hardness ~ 62 HRC in depth of 1-2 mm
Carburizing is performed in a carbon-enriched medium for about 5...10 hours at about 900 °C
The part is machined, then carburized and then heat treated